Finnish University Team’s New Fuel Cell Manufacturing Method Cuts Catalyst Cost 60%
December 22nd, 2011 | by Andrew
Researchers at a Finnish university have come up with a means of significantly reducing the cost of manufacturing fuel cells. Using atomic layer deposition (ALD), the team's new method doesn't require expensive platinum, and requires less than half the amount of catalyst currently used methods require